Material Notes:
Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. MM288 is designed for use as the center web of a triplex lamination. The treated surface offers good compatibility with adhesives and cohesives (cold seals).Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Excellent gas barrierExcellent moisture barriersExcellent light barrierEnhances puncture resistance of the packageFeatures: Flavor & Aroma BarrierGas BarrierGrease ResistantLight BarrierMoisture BarrierOxygen BarrierPuncture ResistantTwo Side ProcessableApplications: Crisps and SnacksDry Foods and Beverage Powders Pet Food Uses: HFFS Flexible PackagingLidding – Flexible Packaging Pouches – Flexible Packaging Pre-made Bags – Flexible PackagingVFFS Flexible PackagingProcessing Method: Cold Seal Adhesive and Inner Web Adhesive LaminationInformation provided by ExxonMobil
Physical Properties Metric English Comments
Water Vapor Transmission 0.101 g/m²/day

@Temperature 38.0 °C
0.00650 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
Oxygen Transmission Rate 15.1 cc/m²/day

@Temperature 23.0 °C
0.970 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
Thickness 15.0 microns
0.590 mil
ExxonMobil Method
Coating Weight 13.4 g/m²
8.40 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.50 GPa
363 ksi
MD; ExxonMobil Method
4.50 GPa
653 ksi
TD; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 3.0 %

@Temperature 135 °C,
Time 432 sec
3.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 3.0 %

@Temperature 135 °C,
Time 432 sec
3.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Optical Properties Metric English Comments
Optical Density 2.9
2.9
ExxonMobil Method
Descriptive Properties Value Comments
Yield 51500 in2/lb