Material Notes:
Product Description: A matte finish, coated, white, polypropylene film designed for use in demanding thermal transfer, pressure-sensitive label applications. It is also compatible with a wide range of water-based or solvent-based flexo, gravure, UV screen, and UV flexo ink systems. The adhesive side is coated to provide improved pressure-sensitive adhesive anchorage.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, North America and South AmericaKey Features: Excellent print resolution and abrasion resistanceWide compatibility with thermal transfer ribbonsExcellent car code scannabilityExcellent static resistant propertiesFeatures:Static Resistant CoatedStatic Resistant Matte CoatedApplications: Household and DetergentsIndustrialPaper Ream wrapPharmaceuticalsUses: Pressure Sensitive LabelsProcessing Method: Digital Offset (HP Indigo) Printing, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, Thermal Transfer Printing, UV Flexographic Printing, UV Screen Printing and Water-based Flexographic PrintingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
ExxonMobil Method
Coating Weight 52.8 g/m²
33.0 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 190 %
190 %
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 50 %
50 %
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, MD 84.8 MPa
12300 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 161 MPa
23300 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 3.9 %

@Temperature 135 °C
3.9 %

@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 3.3 %

@Temperature 135 °C
3.3 %

@Temperature 275 °F
ExxonMobil Method
Optical Properties Metric English Comments
Gloss 8.0 %
8.0 %
45°, Print Surface; ExxonMobil Method
Transmission, Visible 17 %
17 %
ExxonMobil Method
Descriptive Properties Value Comments
Opacity 90
Stiffness (Gurley) 29 mgf
MD
40 mgf
TD
Yield 13410 in2/lb