ExxonMobil Label-Lyte™ 60LH538 OPP Film

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte™ 60LH538 OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A super white opaque polypropylene film face stock with a proprietary caviated core providing high yield and excellent opacity. The coated print surface provides exceptional ink adhesion with a broad range of ink systems. A matte adhesive receptive coating offers excellent anchorage with most pressure sensitive adhesive formulations. 60LH538 is designed for use in pressure sensitive labeling applications where excellent appearance and graphics are desired.Availability: Africa & Middle East, Asia Pacific, Latin America, South America and EuropeKey Features:Excellent whiteness and opacityExcellent compatibility with a broad range of ink systems, including UV flexoExcellent adhesive anchorageExcellent “in-to-out” blocking resistanceExcellent stiffness for automatic label dispensing Features:Adhesive Receptive CoatedHumidity ResistantPasteurizable Print Receptive Coated Applications: Beverage, AlcoholicBeverage, Carbonated Beverage, Mineral WatersBiscuits/Cookie/CrackersConfectionery, Chocolate Confectionery, Gum Confectionery, Sugar Dairy Products Health and Beauty CareHousehold and DetergentsIndustrialPet FoodPharmaceuticals Uses: Pressure Sensitive LabelsProcessing Method: Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, Thermal Transfer Printing, UV Flexographic Printing, UV Letterpress Printing, UV Offset Lithography Printing, UV Screen Printing and Water-based Flexographic PrintingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Thickness 61.0 microns
2.40 mil
ExxonMobil Method
Coating Weight 44.6 g/m²
27.9 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 170 %
170 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 55 %
55 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 1.60 GPa
232 ksi
MD; ExxonMobil Method
2.60 GPa
377 ksi
TD; ExxonMobil Method
Film Tensile Strength at Break, MD 100 MPa
14500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 195 MPa
28300 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 4.0 %

@Temperature 135 °C,
Time 432 sec
4.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 2.0 %

@Temperature 135 °C,
Time 432 sec
2.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Optical Properties Metric English Comments
Gloss 63 %
63 %
45°, Print Surface; ExxonMobil Method
Transmission, Visible 20 %
20 %
ExxonMobil Method
Descriptive Properties Value Comments
Yield 15500 in2/lb