Material Notes:
Product Description: A clear, two-side coated, polypropylene label face stock designed for demanding pressure sensitive applications where outstanding ink adhesion and adhesive anchorage are required. This premium film provides a no label look and is commonly used in beverage, health and beauty, and pharmaceutical applications. The coated print surface is compatible with UV, flexo, letterpress, screen and offset systems. Additionally, it is compatible with solvent and water based flexo and solvent based gravure. 50LL539 is also compatible with hot stamping and cold foil stamping systems. The adhesive side is coated to provide improved anchorage of pressure-sensitive adhesives.Availability: Africa & Middle East, Asia Pacific, Latin America, South America and EuropeKey Features:Excellent gloss and transparencyExcellent compatibility with a broad range of ink systems, including UV flexoExcellent adhesive anchorageExcellent “in-to-out” blocking resistanceExcellent stiffness for automatic label dispensingApplications: Beverage, AlcoholicBeverage, Carbonated Beverage, Mineral WatersBiscuits/Cookie/CrackersConfectionery, Chocolate Confectionery, Gum Confectionery, Sugar Dairy ProductsHealth and Beauty CareHousehold and DetergentsIndustrialPet FoodPharmaceuticalsUses: Pressure Sensitive LabelsProcessing Method: Inner Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, Thermal Transfer Printing, UV Flexographic Printing, UV Letterpress Printing, UV Offset Lithography Printing, UV Screen Printing and Water-based Flexographic PrintingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
ExxonMobil Method
Coating Weight 45.4 g/m²
28.4 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 175 %
175 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 65 %
65 %
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Modulus of Elasticity 2.00 GPa
290 ksi
MD; ExxonMobil Method
3.50 GPa
508 ksi
TD; ExxonMobil Method
Film Tensile Strength at Break, MD 120 MPa
17400 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 245 MPa
35500 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 4.0 %

@Temperature 135 °C,
Time 432 sec
4.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 2.0 %

@Temperature 135 °C,
Time 432 sec
2.0 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Optical Properties Metric English Comments
Haze 2.5 %
2.5 %
ExxonMobil Method
Gloss 80 %
80 %
45°, Print Surface; ExxonMobil Method
Descriptive Properties Value Comments
Yield 15200 in2/lb