ExxonMobil Label-Lyte® 155 LL-434 Coated, Clear OPP Facestock

Category Polymer , Adhesive , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte® 155 LL-434 Coated, Clear OPP Facestock.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Coated, clear, polypropylene label facestock designed for pressure-sensitive applications. This film is ideal for glass bottle labeling applications and provides a "no label" look. It is suitable for wet environments, and may be exposed to a brad range of temperatures, including pasteurizing conditions. The coated print surface provides generally good ink adhesion with UV flexo, UV screen, and water-based and solvent based flexo ink systems. The adhesive side is corona-treated for good pressure-sensitive adhesive anchorage.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Coating Weight >= 44.6 g/m²
>= 27.9 lb/ream
520
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 185 %
185 %
510
Film Elongation at Break, TD 60 %
60 %
510
Film Tensile Strength at Break, MD 114 MPa
16500 psi
510
Film Tensile Strength at Break, TD 231 MPa
33500 psi
510
Thermal Properties Metric English Comments
Shrinkage, MD 3.5 %
3.5 %
at 275°F; 438
Shrinkage, TD 3.5 %
3.5 %
at 275°F; 438
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
444
Gloss 98 %
98 %
442
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Gurley Stiffness, MD, mgf 12
Gurley Stiffness, TD, mgf 22
Wetting Tension, receding COS theta 0.83
Yield, in2/lb 15500