ExxonMobil LLDPE LL 6100.17 Linear Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 6100.17 Linear Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 6100 is a narrow molecular weight butane copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in freezer applications for food packaging.Availability: Latin America, North America and South America Applications: Closures and DispensersHousewaresProtective CapsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ExxonMobil method
ESCR 10% Igepal® 330 hour
330 hour
F50; ASTM D1693B
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.7 MPa
1700 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 0.427 GPa
62.0 ksi
2% Secant; ASTM D638
Flexural Modulus, 1% Secant 483 MPa
70000 psi
ASTM D638
Thermal Properties Metric English Comments
Melting Point <= 255 °C
<= 491 °F
Peak Melting Point; ExxonMobil method