Material Notes:
Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrusion FilmsDiaper BacksheetEmbossed FilmFoamsHygiene PackagingLabel FilmOverwrap FilmPaper OverwrapInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.931 g/cc
0.0336 lb/in³
ExxonMobil method
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 17.2 MPa
2500 psi
ASTM D882
Film Elongation at Break, MD 380 %
380 %
ASTM D882
Film Elongation at Break, TD 600 %
600 %
ASTM D882
Elmendorf Tear Strength MD 150 g
150 g
ASTM D1922
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
Dart Drop Test 70.0 g
0.154 lb
ASTM D1709A
Film Tensile Strength at Break, MD 29.0 MPa
4200 psi
ASTM D882
Film Tensile Strength at Break, TD 24.1 MPa
3500 psi
ASTM D882
1% Secant Modulus, MD 338 MPa
49000 psi
ASTM D882
1% Secant Modulus, TD 379 MPa
55000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 241 °C
<= 466 °F
Peak Melting Point; ExxonMobil method