ExxonMobil Jayflex™ 220 Aliphatic Hydrocarbon Plasticizer

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Exxon Chemical
Trade Name Jayflex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Jayflex™ 220 Aliphatic Hydrocarbon Plasticizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaCAS Number: 64742-47-8Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.780 - 0.830 g/cc
0.0282 - 0.0300 lb/in³
ASTM D4052
Maximum Moisture Content 0.10
0.10
ISO 12937
Descriptive Properties Value Comments
Color >30
Saybolt Units, ASTM 6045 or ASTM D156