ExxonMobil Iotek® 7610 Zinc Ionomer  (discontinued **)

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Iotek® 7610 Zinc Ionomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A low melt index zinc ionomer made from an ethylene acrylic acid base polymer. It is designed to have high durability, resilience and impact strength.Applications: Injection molding; Sheet extrusion.
Physical Properties Metric English Comments
Density 0.964 g/cc
0.0348 lb/in³
Exxon Method
Melt Flow 0.90 g/10 min
0.90 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength, Ultimate 24.0 MPa
3480 psi
ASTM D638
Elongation at Break 470 %
470 %
ASTM D638
Flexural Modulus 0.150 GPa
21.8 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 86.0 °C
187 °F
Exxon Method
Vicat Softening Point 61.0 °C
142 °F
Rate B; ASTM D-1525