Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Iotek® 7030 Zinc Ionomer Molding/Extrusion Resin  (discontinued **)

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Iotek® 7030 Zinc Ionomer Molding/Extrusion Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glass, metals and paper.Applications: Golf ball covers; Injection molded articles; Foams; Impact modifiers.
Physical Properties Metric English Comments
Density 0.964 g/cc
0.0348 lb/in³
Exxon Method
Melt Flow 2.5 g/10 min
2.5 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
ASTM D2240
Tensile Strength, Ultimate 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 460 %
460 %
ASTM D638
Flexural Modulus 0.155 GPa
22.5 ksi
ASTM D790
Tensile Impact Strength 480 kJ/m²
228 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 85.0 °C
185 °F
Exxon Method
Vicat Softening Point 60.0 °C
140 °F
Rate B; ASTM D-1525
Users viewing this material also viewed the following: