ExxonMobil HDPE HD 6601.29 High Density Polyethylene Copolymer Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HDPE HD 6601.29 High Density Polyethylene Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HD 6601 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance. Ideally suited for articles requiring rugged physical performance in cold temperature environments.Availability: Latin America, North America and South America Additive: Long Term UV-15 Stabilizer: YesApplications: Automotive ComponentsIndustrial ClosuresRecreation Vehicle – ComponentsWaste CartsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ExxonMobil method
ESCR 10% Igepal® 10 hour
10 hour
F50; ASTM D1963B
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.896 MPa
130 psi
ASTM D638
Tensile Strength, Yield 22.8 MPa
3300 psi
ASTM D638
Flexural Modulus, 1% Secant 758 MPa
110000 psi
ASTM D790B
Izod Impact, Notched 0.486 J/cm

@Temperature -40.0 °C
0.910 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point <= 266 °C
<= 511 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 66.7 °C
152 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.2 °C
108 °F
ASTM D648B