Material Notes:
A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applications. This grade of Geolast TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Recyclable. Designed for improved fluid resistanceInformation provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
.12 in; ASTM D2240
46
46
Air at 257°F, 168 hr; ASTM D573
Tensile Strength at Break 17.0 MPa
2470 psi
Across Flow; ASTM D412
17.541 MPa
2544.1 psi
Air at 257°F, 168 hr; ASTM D573
Tensile Strength, Ultimate 11.3 MPa
1640 psi
Across Flow; ASTM D412
Elongation at Break 303.4 %
303.4 %
Air at 257°F, 168 hr; ASTM D573
370 %
370 %
Across Flow; ASTM D412
Tear Strength 87.1 kN/m
497 pli
73°C, Die C; ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -27.2 °C
-17.0 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Melt Temperature <= 102 °C
<= 215 °F
Descriptive Properties Value Comments
Change in Mass in IRM 903 Oil at 257°F for 70 hr 0.41
Color Black
Form Pellets