Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ LNU 012 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ LNU 012 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin with good heat resistance and good surface finish designed for fast injection molding of large electrical appliance parts.Availability: Africa & Middle East, Asia Pacific, Europe, North America and South America Features:Good Mold ReleaseGood Surface Finish Uses: Appliance ComponentsAppliances Consumer ApplicationsProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ISO 1183
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 2.20 GPa
319 ksi
Secant; ISO 527-2
Flexural Modulus 2.25 GPa
326 ksi
Secant; ISO 178
Charpy Impact, Notched 0.252 J/cm²

@Temperature 22.8 °C
1.20 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 57.8 °C
136 °F
ISO 75-2/A
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved