Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ HMU 405 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ HMU 405 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin with high heat ageing resistance, high transparency, low color and low discoloration for contact with hot water, hot air and detergent in electrical appliances such as washing machines.Availability: Latin America, North America and South America Features:Good Mold ReleaseGood Surface FinishGood Thermal Stability Uses: Appliance ComponentsAppliancesAutomotive ApplicationsAutomotive Under the HoodConsumer ApplicationsProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
ISO 527-2/50
Elongation at Break 4.0 %
4.0 %
ISO 527-2/50
Elongation at Yield 3.0 %
3.0 %
ISO 527-2/50
Tensile Modulus 4.50 GPa
653 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.294 J/cm²

@Temperature 22.8 °C
1.40 ft-lb/in²

@Temperature 73.0 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
279 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75-2/A
Users viewing this material also viewed the following: