Material Notes:
Availability: North America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.775 g/cc

@Temperature 15.6 °C
0.0280 lb/in³

@Temperature 60.0 °F
ASTM D4052
Kinematic Viscosity 1.27 cSt
1.27 cSt
ASTM D445
Vapor Pressure <= 0.00267 bar

@Temperature 20.0 °C
<= 2.00 torr

@Temperature 68.0 °F
ExxonMobil Method
Thermal Properties Metric English Comments
Boiling Point 161 °C
322 °F
Initial; ASTM D86
Flash Point 43.9 °C
111 °F
ASTM D93
Descriptive Properties Value Comments
Aniline Point 153°F
Method E, ASTM D611
Aromatic Content 0.0004
ExxonMobil Method
Dry Point 352°F
ASTM D86