ExxonMobil Exxon™ 4266 Star-Branched Butyl

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Exxon Chemical
Trade Name Exxon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxon™ 4266 Star-Branched Butyl.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Exxon SB Butyl is a copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
Mooney Viscosity 34 - 44

@Temperature 125 °C
34 - 44

@Temperature 257 °F
ML 1 + 8; ASTM D1646
Processing Properties Metric English Comments
Cure Time 2.50 - 5.50 min
0.0417 - 0.0917 hour
ts2; ASTM D2084
6.00 - 12.0 min
0.100 - 0.200 hour
t`50; ASTM D2084
21.0 - 29.0 min
0.350 - 0.483 hour
t`90; ASTM D2084
Descriptive Properties Value Comments
Anti oxidant >.05%
wt %
cure MH 69 ± 6
dN.m
cure ML 11.5 ± 4.5
dN.m
Water <.3%
wt %