Material Notes:
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber bales.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
Mooney Viscosity 41 - 51

@Temperature 125 °C
41 - 51

@Temperature 257 °F
ML 1 + 8; ASTM D1646
46

@Temperature 125 °C
46

@Temperature 257 °F
ML 1 + 8, Target; ASTM D1646
Maximum Moisture Content 0.30
0.30
Component Elements Properties Metric English Comments
Calcium, Ca 0.12 %
0.12 %
Target
0.080 - 0.16 %
0.080 - 0.16 %
Processing Properties Metric English Comments
Cure Time 1.00 - 6.00 min
0.0167 - 0.100 hour
ts2; ASTM D2084
3.50 min
0.0583 hour
ts2, Target; ASTM D2084
6.00 min
0.100 hour
t`50, Target; ASTM D2084
3.00 - 9.00 min
0.0500 - 0.150 hour
t`50; ASTM D2084
9.00 min
0.150 hour
t`90, Target; ASTM D2084
5.00 - 13.0 min
0.0833 - 0.217 hour
t`90; ASTM D2084
Descriptive Properties Value Comments
Antioxidant 0.02-0.12%
non-staining
Bromine 0.93-1.23%
1.08%
cure MH 38-52 dN.m
45 dN.m
Target
cure ML 13.5-22.5 dN.m
18 dN.m
Target
stabilizer (epoxidized soybean oil) 1.3 ± 0.3%
1.3%