ExxonMobil Exxelor™ VA 1202 Low Viscosity Ethylene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , Anhydride-Modified Polyethylene
Manufacturer Exxon Chemical
Trade Name EXXELOR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxelor™ VA 1202 Low Viscosity Ethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exxelor VA 1202 polymer resin is a low viscosity ethylene copolymer functionalized with maleic anhydride by reactive extrusion. Its fully saturated backbone results in outstanding thermal and oxidative stability, leading to good weatherability. This grade is designed for:Super-tough nylon applications without low temperature impact requirements.Medium-low toughness applications.Glass-filled impact modified applications.Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ExxonMobil Method
Volatiles <= 0.15 %
<= 0.15 %
AM-S 350.03
Melt Flow 17 g/10 min

@Load 5.00 kg,
Temperature 230 °C
17 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Optical Properties Metric English Comments
Yellow Index <= 20 %
<= 20 %
ASTM E313
Descriptive Properties Value Comments
Maleic anhydride graft level High
FTIR EPK-04 QT-02