Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxelor™ PE 1040 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , Anhydride-Modified Polyethylene
Manufacturer Exxon Chemical
Trade Name EXXELOR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxelor™ PE 1040 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exxelor PE 1040 polymer resin is a maleic anhydride functionalized high density polyethylene, produced by reactive extrusion. It has been primarily designed to act as a coupling agent or tie layer in multilayer polyethylene compounds, or as a coupling agent or tie layer in multilayer polyethylene systems to ensure compatibility and improve adhesion of the different layers. This grade is designed to:Function as a coupling agent between reinforcing materials such as natural and mineral fillers and high density polyethylene to improve mechanical properties.Achieve compatibility and adhesion between high density polyethylene and polyamide.Function as a tie layer in multilayer tank systems with high density polyethylene and a barrier layer.Key Features: Performance enhancements in natural and mineral filled:Improved mechanical properties.Improved notched Izod and Charpy impact strength.Reduced water absorption.Adhesion as a tie layer in polyethylene based multilayer tank systems.Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ExxonMobil Method
Volatiles <= 0.15 %
<= 0.15 %
AM-S 350.03
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 and ISO 1133
3.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238 and ISO 1133
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
Peak; ExxonMobil Method
Optical Properties Metric English Comments
Yellow Index <= 10 %
<= 10 %
ASTM E313
Descriptive Properties Value Comments
Maleic anhydride graft level High
FTIR EPK-04 QT-02
Users viewing this material also viewed the following: