ExxonMobil Escorene® UL-7840C EVA Copolymer, Adhesive and Sealant Grade  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® UL-7840C EVA Copolymer, Adhesive and Sealant Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
Exxon Method
Apparent Bulk Density 0.577 g/cc
0.0208 lb/in³
ASTM D1895 (B)
Viscosity 1400 cP

@Temperature 121 °C
1400 cP

@Temperature 250 °F
melt viscosity; ASTM D-3236
Melt Flow 43 g/10 min
43 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.00 MPa
435 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 61.0 °C
142 °F
Exxon Method
Vicat Softening Point 105 °C
221 °F
Softening Point, R&B; ASTM E-28