Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® UL 7620 Adhesive Application Resin  (discontinued **)

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® UL 7620 Adhesive Application Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Escorene Ultra UL 7620 is a medium flow rate, 24% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealants and wax blends.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ExxonMobil Method
Vinyl Acetate Content 24 %
24 %
ExxonMobil Method
Melt Flow 112 g/10 min
112 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
15s; ASTM D2240
Hardness, Shore D 23
23
15s; ASTM D2240
Tensile Strength at Break 3.52 MPa
510 psi
ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
Flexural Modulus 0.0314 GPa
4.55 ksi
1% secant; ASTM D790
Thermal Properties Metric English Comments
Melting Point 73.3 °C
164 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 41.1 °C
106 °F
ASTM D1525
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved