Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ UL 00112 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 00112 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: UL 00112 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applications:Agricultural FilmCompounding Thick FilmWire and Cable Compounds Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil method
Vinyl Acetate Content 12 %
12 %
ExxonMobil method
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Film Elongation at Break, TD 600 %
600 %
ASTM D882
Film Tensile Strength at Break, MD 30.3 MPa
4400 psi
ASTM D882
Film Tensile Strength at Break, TD 29.0 MPa
4200 psi
ASTM D882
1% Secant Modulus, MD 103 MPa
15000 psi
ASTM D882
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 205 °C
<= 401 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 79.4 °C
175 °F
ASTM D1525
Users viewing this material also viewed the following: