Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LX-0252 LMDPE Rotational Molding Grade  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LX-0252 LMDPE Rotational Molding Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene providing an excellent processing window for molding toys and consumer items. The resin is formulated to provide intermediate term UV stability.Applications: Toys; Consumer items.
Physical Properties Metric English Comments
Density 0.9355 g/cc
0.03380 lb/in³
Exxon Method
Environmental Stress Crack Resistance 200 hour
200 hour
F50, Condition B; ASTM D-1693
Melt Flow 5.5 g/10 min
5.5 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.3 MPa
2360 psi
ASTM D638
Elongation at Break 405 %
405 %
ASTM D638
Flexural Modulus 0.579 GPa
84.0 ksi
ASTM D790
Impact Test 179 J

@Thickness 6.35 mm,
Temperature -40.0 °C
132 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
Impact Strength; Max Force; ARM
Thermal Properties Metric English Comments
Melting Point 124.8 °C
256.6 °F
Exxon Method
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648