Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® LL-8461 LMDPE Rotational Molding Grade  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LL-8461 LMDPE Rotational Molding Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.LL-8400 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8461 is fully formulated long term UV stability package in ground form.Applications: Septic tanks; Chemical storage bins; Rotomolded pallets; Potable water tanks.
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
Exxon Method
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50, Condition B; ASTM D1693
Melt Flow 3.3 g/10 min
3.3 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.9 MPa
2600 psi
ASTM D638
Elongation at Break 765 %
765 %
ASTM D638
Flexural Modulus 0.668 GPa
96.9 ksi
ASTM D790
Impact Test 237 J

@Thickness 6.35 mm,
Temperature -40.0 °C
175 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
Impact Strength; Max Force; ARM
Thermal Properties Metric English Comments
Melting Point 126.5 °C
259.7 °F
Exxon Method
Deflection Temperature at 0.46 MPa (66 psi) 52.5 °C
127 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved