ExxonMobil Escorene® LD-701 High EVA Film Resin  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-701 High EVA Film Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A fractional melt, 10.5% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness particularly at low temperatures.Applications: Heat seal layer in coextruded or laminated structures; Liquid packaging; Profile extrusions; Frozen food packaging.
Physical Properties Metric English Comments
Density 0.932 g/cc
0.0337 lb/in³
Exxon Method
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F50, Condition A; ASTM D1693
Melt Flow 0.20 g/10 min
0.20 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Hardness, Shore D 39
39
ASTM D2240
Tensile Strength, Ultimate 17.0 MPa
2470 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0960 GPa
13.9 ksi
1% Secant, ASTM D790
Tensile Impact Strength 732 kJ/m²
348 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 96.0 °C
205 °F
Exxon Method
Vicat Softening Point 84.0 °C
183 °F
1000g; ASTM D-1525