Material Notes:
Product Description: Exact 8210 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for seal layers in multilayer film applications requiring good flow/caulking and low SIT. This material can be used in cling layers in blown and cast stretch film..Key Features: Low temperature heat seal performance including low seal initiation temperature and good caulking/flow. Low hexane extractables..Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaAdditive: Thermal Stabilizer This polymer complies with FDA regulation 21 CFR 177.1520 (Olefin polymers), paragraph (c) 3.2c, and may be used as articles or components of articles intended for use in contact with food, except for articles used for packing or holding food during cooking. Finished articles may contact food only under Conditions of Use C through H described in Table 2 of 21 CFR 176.170(c).Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.882 g/cc
0.0319 lb/in³
ISO 1183
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
ISO 868
Thermal Properties Metric English Comments
Melting Point 75.0 °C
167 °F
Peak Melting Temperature; ISO 11357-3
Vicat Softening Point 45.0 °C
113 °F
ISO 306/A
Brittleness Temperature <= -105 °C
<= -157 °F
ASTM D746
Descriptive Properties Value Comments
Features Thermal Stabilizer