Material Notes:
ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable for use as a polymer modifier to improve bonding and toughness.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ExxonMobil Method
Methyl Acrylate Content 6.5 %
6.5 %
Acrylic Acid Content 6.5 %
6.5 %
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Neck In 3.50 cm
1.38 in
at 200 m/min, 35 rpm, 295°C; ExxonMobil Method
3.70 cm
1.46 in
at 100 m/min, 35rpm, 295°C; ExxonMobil Method
Drawdown 3.91 m/s
770 ft/min
at 35 rpm, 295°C; ExxonMobil Method
4.93 m/s
970 ft/min
at 65 rpm, 295°C; ExxonMobil Method
Thermal Properties Metric English Comments
Melting Point 86.1 °C
187 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 61.1 °C
142 °F
ASTM D1525