Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil ENABLE™ EN 33900 Adhesive and Sealant Applications Resin  (discontinued **)

Category Polymer , Adhesive , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil ENABLE™ EN 33900 Adhesive and Sealant Applications Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Enable EN 33900 is a high flow, 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ExxonMobil Method
Viscosity 8340 cP

@Temperature 190 °C
8340 cP

@Temperature 374 °F
ASTM D3236
Butyl Acrylate Content 32.5 %
32.5 %
Mechanical Properties Metric English Comments
Hardness, Shore A 44
44
15s; ASTM D2240
Tensile Strength at Break 0.965 MPa
140 psi
ASTM D638
Elongation at Break 135 %
135 %
ASTM D638
Flexural Modulus 0.00538 GPa
0.780 ksi
1% secant; ASTM D790
Thermal Properties Metric English Comments
Melting Point 60.0 °C
140 °F
Peak Melting Temperature; ExxonMobil Method
Descriptive Properties Value Comments
Features Thermal Stabilizer
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved