Material Notes:
Enable EN 33330 is a high flow, 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ExxonMobil Method
Butyl Acrylate Content 32.5 %
32.5 %
Melt Flow 330 g/10 min
330 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
15s; ASTM D2240
Tensile Strength at Break 1.24 MPa
180 psi
ASTM D638
Elongation at Break 270 %
270 %
ASTM D638
Flexural Modulus 0.00724 GPa
1.05 ksi
1% secant; ASTM D790
Thermal Properties Metric English Comments
Melting Point 61.7 °C
143 °F
Peak Melting Temperature; ExxonMobil Method
Descriptive Properties Value Comments
Features Thermal Stabilizer