ExxonMobil Digilyte® 65 EW-214 Coated, White Opaque OPP Facestock

Category Polymer , Adhesive , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Digilyte®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Digilyte® 65 EW-214 Coated, White Opaque OPP Facestock.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
White, polypropylene, pressure-sensitive, label facestock designed to be printed on an Indigo® Omnius® One-Shot Color™ press. This film offers strength and opacity. The ElectroInk® receptive coating assures excellent anchorage and improved abrasion resistance with the ElectroInk digital printing inks. The opposite surface is coated to provide excellent pressure-sensitive adhesive adhesion.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Thickness 66.0 microns
2.60 mil
Coating Weight >= 47.7 g/m²
>= 29.8 lb/ream
520
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 200 %
200 %
510
Film Elongation at Break, TD 50 %
50 %
510
Film Tensile Strength at Break, MD 84.861 MPa
12308 psi
510
Film Tensile Strength at Break, TD 180.33 MPa
26154 psi
510
Thermal Properties Metric English Comments
Shrinkage, MD 5.0 %
5.0 %
at 275°F; 438
Shrinkage, TD 5.0 %
5.0 %
at 275°F; 438
Optical Properties Metric English Comments
Transmission, Visible 18 %
18 %
417
Descriptive Properties Value Comments
Gurley Stiffness, MD, mgf 23
Gurley Stiffness, TD, mgf 40
Yield, in2/lb 14500