Material Notes:
Primarily used for consumer packaging, VersaTech RPET delivers on excellent clarity and high gloss, while providing good impact and tear resistance properties that are demanded in today’s retail environment. Characteristics:Excellent clarityImpact and tear resistantHigh glossEnd Uses:Consumer packagingInformation provided by Ex-Tech Plastics Inc.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
Viscosity Measurement >= 0.65
>= 0.65
Intrinsic Viscosity; ASTM D3835
Linear Mold Shrinkage 0.020 - 0.050 cm/cm
0.020 - 0.050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.26 - 55.16 MPa
7000 - 8000 psi
ASTM D638
Elongation at Break 100 - 200 %
100 - 200 %
Flexural Modulus 2.07 - 2.41 GPa
300 - 350 ksi
ASTM D790
Optical Properties Metric English Comments
Haze <= 10 %

@Thickness <=0.508 mm
<= 10 %

@Thickness <=0.0200 in
ASTM D1003
Transmission, Visible >= 85 %
>= 85 %
ASTM D1003
Descriptive Properties Value Comments
Clarity >97%
ASTM D1003