Ex-Tech Plastics RenewTech™ BioPlastics Ingeo™ PLA

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polylactic Acid (PLA) Biopolymer
Manufacturer Ex-Tech Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ex-Tech Plastics RenewTech™ BioPlastics Ingeo™ PLA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Derived from annually renewable resources, RenewTech™ BioPlastics 7000 sheet is made with Ingeo™ PLA biopolymer as a base, giving you a packaging solution with competitive cost value performance compared to traditional materials. RenewTech 7000 complies with FDA and European requirements for food packaging.Characteristics:Made from annually renewable resourcesImproved environmental footprint (requires less non-renewable energy and generates significantly less greenhouse gas)Excellent flavor and aroma barrierSuperior print and laminationHigh glossStones allows for down gaugingFood contact approvedSuperior visual qualitiesHigh modulusCompostableEnd Uses:Food packagingOrganic in-store prepared food packagingThermoformed hinged packagingTray packagingInformation provided by Ex-Tech Plastics Inc.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Melt Flow 4.0 - 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 - 8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 53.0 MPa
7690 psi
ASTM D882
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D882
Elongation at Break 6.0 %
6.0 %
ASTM D882
Tensile Modulus 3.50 GPa
508 ksi
ASTM D882
Izod Impact, Notched 0.1281 J/cm
0.2400 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Clarity Transparent