Material Notes:
Manufactured in thickness from 10 to 60 mils, PerformTech XSD-28 is available in rigid vinyl or PET. XSD-28 is a static dissipative sheet engineered specifically for ESD sensitive packaging for use in ESD controlled environments.Characteristics:Engineered for packaging to contain ESD-sensitive items and for use in ESD controlled environments.Static Dissipative range 1 x 105 ohms per square to less than 1 x 1012 ohms per square.Thickness ranging from .010 to .060”End Uses:Thermoformed containers.High level of surface resistance and volume resistivity is ideal for the containment, transport and long-term storage of ICs, printed circuit boards and other ESD-sensitive components.Information provided by Ex-Tech Plastics Inc.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 43.4 MPa
6300 psi
ASTM D882
Elongation at Break >= 100 %
>= 100 %
ASTM D882
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
SOP-MEC-002.01
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 61.7 °C
143 °F
ASTM D648-96
Electrical Properties Metric English Comments
Surface Resistance 1.00e+9 ohm
1.00e+9 ohm
EOS/ESD S11.11-1993
Surface Resistivity per Square 1.00e+10 ohm
1.00e+10 ohm
12% Humidity; ASTM D257
Static Decay <= 2.0 sec
<= 2.0 sec
EIA 541
Descriptive Properties Value Comments
12 day oven again 4.7e10 Ohms
ASTM D257
Cold Impact -35°C
ASTM D1790
Contact Corrosivity no corrosion
FTM 101C
Gauge Tolerance +/-5%
gamma or beta gauges
Polycarbonate Compatibility no attack
EIA 564
Tribocharging <0.13 nC/in2