Material Notes:
Description: PLEXIGLAS® GS cast acrylic has the following properties:absolutely colorless and clearbreak-resistantunequalled resistance to weathering and ageinghigh-quality surface and planarity; brilliant or satin (PLEXIGLAS SATINICE®)sheets, blocks, tubes, round and square rods2 to 160 mm solid sheet / block thicknessstandard size up to 3050 x 2030 mmmore than 50 standard colorsgood resistance to dilute acidslimited resistance to organic solventsgood resistance to alkalisvery easy to work, similar to hardwoodeasy to thermoform over wide range of conditionseasily and firmly bonded, e.g. with reaction adhesives (e.g. ACRIFIX® 190, 192)burns more or less like hardwood; very little smoke generationmax. service temperature approx. 80 °CSpecific Notes for this Material: UV-absorbing solid sheet special grade, flame retarded with integrated PA threads, corresponds to ZTV-Lsw 88, EN 1793 and EN 1794 for noise control barriers.Information provided by degussa.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ISO 527
Modulus of Elasticity 3.30 GPa
479 ksi
ISO 527
Flexural Strength >= 98.0 MPa
>= 14200 psi
ISO 178
Fatigue Strength 38.0 MPa
5510 psi
Alternating Bending Strength (Unnotched Specimen); ISO 4137
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
DIN 53752A
Vicat Softening Point 110 °C
230 °F
ISO 306
Optical Properties Metric English Comments
Transmission, Visible 50 %
50 %
Midnight Blue Grade; DIN 53752-A
51 %
51 %
Smokey Brown Grade; DIN 53752-A
56 %
56 %
Sky Blue Grade; DIN 53752-A
57 %
57 %
Sea Green Grade; DIN 53752-A
60 %
60 %
Steel Blue Grade; DIN 53752-A
62 %
62 %
Forest Green Grade; DIN 53752-A
83 %
83 %
Spring Green Grade; DIN 53752-A
92 %
92 %
Clear Grade; DIN 53752-A
Electrical Properties Metric English Comments
Shielding Effectiveness 30 dB

@Thickness 15.0 mm
30 dB

@Thickness 0.591 in
Weighted Sound Reduction Index; EN 1793-2, ZTV-Lsw 88
32 dB

@Thickness 20.0 mm
32 dB

@Thickness 0.787 in
Weighted Sound Reduction Index; EN 1793-2, ZTV-Lsw 88
33 dB

@Thickness 25.0 mm
33 dB

@Thickness 0.984 in
Weighted Sound Reduction Index; EN 1793-2, ZTV-Lsw 88
Copyright © lookpolymers.com All Rights Reserved