Evonik Corporation Plexiglas® 99524 Film Crystal Clear Elastomer Based Film

Category Polymer , Film , Thermoplastic , Acrylic (PMMA)
Manufacturer Evonik Corporation
Trade Name Plexiglas®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Evonik Corporation Plexiglas® 99524 Film Crystal Clear Elastomer Based Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: PLEXIGLAS® Film 99524, based on polymethyl methacrylate and polybutyl acrylate elastomer, is absolutely crystal-clear. The film shows very good performance during long-term outdoor weathering. Its high-gloss surface is immaculate ("Class A" surface). The film also shows very good abrasion resistance as well as resistance to weak acids and non-polar solvents. To be added to all this are outstanding performance in die-cutting and very good behavior in all forming processes.Specific Notes for this Material: PLEXIGLAS® Film Clear 99524 is suitable for decorative and protective surfacing of injection molded automotive body parts, items used in telecommunications and of domestic appliances. It can be easily processed by insert molding.Information provided by degussa.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 54.0 MPa
7830 psi
no direction given; ISO 527
Film Elongation at Break, MD 35 %
35 %
no direction given; ISO 527
Film Elongation at Yield, MD 5.0 %
5.0 %
no direction given; ISO 527
Tensile Modulus 2.20 GPa
319 ksi
ISO 527
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C

@Temperature 0.000 - 50.0 °C
55.6 µin/in-°F

@Temperature 32.0 - 122 °F
DIN 53752A
Specific Heat Capacity 1.50 J/g-°C
0.359 BTU/lb-°F
Vicat Softening Point 100 °C
212 °F
ISO 306, Method B 50
Optical Properties Metric English Comments
Haze <= 0.60 %
<= 0.60 %
ASTM D1003
Yellow Index <= 0.40 %
<= 0.40 %
ASTM D1925
Transmission, Visible 92 %
92 %
DIN 5036
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
No thickness given; IEC 250
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
IEC 250
Descriptive Properties Value Comments
Pencil Hardness 2H
ASTM D3363