Material Notes:
A saturated, linear copolyester, slightly crystalline. Generally used in a solution, film or melt from heated tanks or extruders for the adhesion of aluminum, PET, PVC, ABS, copper, paper, cardboard, leather and fabric
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
DIN 53 479
Viscosity 15000 cP

@Temperature 220 °C
15000 cP

@Temperature 428 °F
melt; (Plate/Plate)
25000 cP

@Temperature 200 °C
25000 cP

@Temperature 392 °F
melt; (Plate/Plate)
40000 cP

@Temperature 180 °C
40000 cP

@Temperature 356 °F
melt; (Plate/Plate)
80000 cP

@Temperature 160 °C
80000 cP

@Temperature 320 °F
melt; (Plate/Plate)
Viscosity Test 75 - 85 cm³/g
75 - 85 cm³/g
DIN 53 728
Melt Flow 110 g/10 min

@Temperature 160 °C
110 g/10 min

@Temperature 320 °F
DIN ISO 1133
190 g/10 min

@Temperature 180 °C
190 g/10 min

@Temperature 356 °F
DIN ISO 1133
290 g/10 min

@Temperature 200 °C
290 g/10 min

@Temperature 392 °F
DIN ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 19
19
Tensile Strength, Ultimate 5.00 MPa
725 psi
DIN EN ISO 527-1/3
Elongation at Break 800 %
800 %
Thermal Properties Metric English Comments
Melting Point 80.0 - 95.0 °C
176 - 203 °F
optical; Mettler FP 82
Softening Point 100 °C
212 °F
DIN ISO 4625
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
DIN 53 765
Chemical Properties Metric English Comments
Total Acid Number <= 3.0
<= 3.0
DIN EN ISO 2114
Descriptive Properties Value Comments
Hydroxyl Number (mg KOH/g) 4-10
DIN 53 240-2