Evonik Corporation DYNAPOL® LH 818 Polyester Resin

Category Polymer , Thermoset , Polyester, TS
Manufacturer Evonik Corporation
Trade Name DYNAPOL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Evonik Corporation DYNAPOL® LH 818 Polyester Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
These coating raw materials are suitable for the production of coatings with very good adhesion offering an optimum of elasticity and formability together with an excellent surface hardness. For this reason, lacquers based on DYNAPOL® have proved particularly suitable for stampable and deep drawable coatings. A wide range of products is available for various requirements of the paint and coating industry. DYNAPOL® polyester resins are mainly used for stoving enamels in combination with amino resins. Special properties, such as chemical resistance, weathering resistance and elasticity, can be improved by using blocked polyisocyanate resins. Stoving enamels based on high-molecular copolyesters show particularly good mechanical properties. Medium and low-molecular polyester resins containing more hydroxyl groups are suitable for the manufacture of stoving enamels with good reactivity and high solids content. In combination with high-molecular copolyesters the quality of films can be optimized.
Physical Properties Metric English Comments
Molecular Weight 6000 g/mol
6000 g/mol
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 35.0 °C
95.0 °F
Chemical Properties Metric English Comments
Total Acid Number 1.0
1.0
[mg KOH/g]
Descriptive Properties Value Comments
Hydroxyl Number (mg KOH/g) 20