Evonik Corporation 853-2010 ACRYLIC Urethane Industrial Colorant

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Evonik Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Evonik Corporation 853-2010 ACRYLIC Urethane Industrial Colorant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionThe 853 Acrylic Urethane line is based upon an acrylic polyol, which is reactive with aliphatic isocyanates. It is designed specifically for two-package urethanes used in heavy duty maintenance applications such as chemical plant storage tanks and offshore rigs and platforms. Polyurethane coatings tinted with 853 colorants should have excellent hardness, resistance properties, and durability. Although the Chroma-Chem® 844 colorants can also be used in two-package urethanes, the 853 line gives particularly good performance in highly corrosive atmospheres or where coatings are subjected to extremely rough treatment.
Physical Properties Metric English Comments
Specific Gravity 2.14 g/cc
2.14 g/cc
Solids Content 12.6 %
12.6 %
vehicle
65 %
65 %
pigment
Volatile Organic Compounds (VOC) Content 480 g/l
480 g/l
Volatiles 22.4 %
22.4 %
solvent
Descriptive Properties Value Comments
Colorant Medium Chrome Yellow
OH milli equivalent weights 13.32
per 1 fl. Oz of colorant
21
per 100 grams of colorant
Pigment Dominion 1003