Evonik CYRO XT® Polymer 2000-5052 Acrylic-Based Multipolymer Molding Compound

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Optical Grade, Molded
Manufacturer Evonik CYRO
Trade Name XT® Polymer
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Evonik CYRO XT® Polymer 2000-5052 Acrylic-Based Multipolymer Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by CYRO IndustriesUses: molding applications where clarity, gloss, toughness, and resistance to fatty acids are of primary importance.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Viscosity 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 240 °C
2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 464 °F
Approximate value
Melt Flow 4.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
4.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Spiral Flow 74.0 cm
29.1 in
215°C; 1/4 in half round channel
Mechanical Properties Metric English Comments
Hardness, Rockwell M 60
60
ASTM D785
Tensile Strength, Ultimate 61.0 MPa
8850 psi
ASTM D638
Elongation at Break 11 %
11 %
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Tensile Modulus 3.40 GPa
493 ksi
ASTM D638
Flexural Yield Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm

@Diameter 6.35 mm
0.806 ft-lb/in

@Diameter 0.250 in
bar; ASTM D256
Thermal Properties Metric English Comments
Specific Heat Capacity 1.30 J/g-°C

@Temperature 25.0 °C
0.311 BTU/lb-°F

@Temperature 77.0 °F
1.90 J/g-°C

@Temperature 100 °C
0.454 BTU/lb-°F

@Temperature 212 °F
2.30 J/g-°C

@Temperature 175 °C
0.550 BTU/lb-°F

@Temperature 347 °F
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
181 °F
ASTM D648
Vicat Softening Point 94.0 °C
201 °F
ASTM D1525
Oxygen Index 17.2 %
17.2 %
ASTM D2863
Optical Properties Metric English Comments
Refractive Index 1.515
1.515
ASTM D542
Haze 4.0 %
4.0 %
ASTM D1003
Transmission, Visible 84 %
84 %
ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 216 - 249 °C
421 - 480 °F
Copyright © lookpolymers.com All Rights Reserved