Evonik CYRO MHOROMER® BM 903 2-Hydroxyethyl Methacrylate

Category Polymer , Thermoset , Methacrylate
Manufacturer Evonik CYRO
Trade Name MHOROMER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Evonik CYRO MHOROMER® BM 903 2-Hydroxyethyl Methacrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Adhesion promoter for polymers. Thermosetting paints. Hydrophilic polymers. Light-curing polymer systems.Appearance: Clear, colorless liquid.Odor: Ester-likeCAS: 868-77-9Information Provided by Evonik CYRO
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Viscosity 5.0 cP

@Temperature 30.0 °C
5.0 cP

@Temperature 86.0 °F
Molecular Weight 130.1 g/mol
130.1 g/mol
Vapor Pressure 0.000100 bar

@Temperature 20.0 °C
0.0750 torr

@Temperature 68.0 °F
Thermal Properties Metric English Comments
Boiling Point 250 °C

@Pressure 0.1013 MPa
482 °F

@Pressure 14.69 psi
Flash Point 101 °C
214 °F
DIN 51758
Optical Properties Metric English Comments
Refractive Index 1.453

@Temperature 20.0 °C
1.453

@Temperature 68.0 °F
Chemical Properties Metric English Comments
Acid Value <= 1.5
<= 1.5
Rohm Method: M4 (acid-base titr., MAAC)
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
Rohm Method: M3 (according to K. Fischer)
Descriptive Properties Value Comments
Color max. 30
Rohm Method: M5 (Pt-Co)
Degree of Purity (%) min. 97
Rohm Method: M2-8 (GC)
Ethyleneglycol dimethacrylate (%) max. 0.2
Rohm Method: M2-8 (GC)
Heat of Polymerization (kJ/mol) 50
MEHQ 180-220
ppm, Rohm Method: M1-1 (HPLC), MEHQ
Polyethyleneglycol monomethacrylates (%) max. 1.3
Rohm Method: M2-8 (GC)
Solidification Point (°C) below -60
Solubility (%) miscible with water in any ratio