Evonik CYRO Acrylite Plus® zk5HF Impact Acrylic Polymer

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Impact Modified, Molded
Manufacturer Evonik CYRO
Trade Name ACRYLITE PLUS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Evonik CYRO Acrylite Plus® zk5HF Impact Acrylic Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Bulk Density 0.710 g/cc
0.0257 lb/in³
ASTM D1895
Water Absorption <= 0.30 %
<= 0.30 %
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D951
Melt Flow 14.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
14.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 82
82
ASTM D785
Tensile Strength at Break 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 7.5 %
7.5 %
ASTM D638
Elongation at Yield 4.3 %
4.3 %
ASTM D638
Tensile Modulus 2.38 GPa
345 ksi
ASTM D638
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 2.17 GPa
315 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm

@Diameter 6.35 mm
0.750 ft-lb/in

@Diameter 0.250 in
BAR; ASTM D256
0.304 J/cm

@Diameter 6.35 mm,
Temperature 0.000 °C
0.570 ft-lb/in

@Diameter 0.250 in,
Temperature 32.0 °F
BAR; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C

@Thickness 6.35 mm
194 °F

@Thickness 0.250 in
Annealed; ASTM D648
Vicat Softening Point 96.1 °C
205 °F
ASTM D1525
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D542
Haze 1.3 %
1.3 %
ASTM D1003
Yellow Index -0.700 %
-0.700 %
ASTM E313
Transmission, Visible 89 %
89 %
ASTM D1003
Processing Properties Metric English Comments
Middle Barrel Temperature 232 - 249 °C
450 - 480 °F
Cylinder Temp
Melt Temperature 232 - 249 °C
450 - 480 °F
Mold Temperature 43.3 - 82.2 °C
110 - 180 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 3 - 4 hour
3 - 4 hour