Material Notes:
ACRYLITE® SuPure™ acrylic polymer is an exceptional pure polymer designed for applications that demand maximum cleanliness. Our proprietary purification process starts at CYRO’s manufacturing plant and extends all the way to your facility’s processing point – for a total purity solution. It ensures a polymer free of dust, fines and contaminants that consistently delivers exceptional clarity and eliminates costly defects.Information provided by Cyro Industries
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Water Absorption <= 0.30 %
<= 0.30 %
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D551
Melt Flow 6.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93
93
ASTM D785
Tensile Strength, Yield 72.0 MPa
10400 psi
ASTM D638
Elongation at Break 4.0 - 6.0 %
4.0 - 6.0 %
ASTM D638
Elongation at Yield 4.0 - 6.0 %
4.0 - 6.0 %
ASTM D638
Tensile Modulus 3.00 GPa
435 ksi
ASTM D638
Flexural Strength 111.7 MPa
16200 psi
ASTM D790
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Izod Impact, Notched 0.192 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.360 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 97.8 °C
208 °F
ASTM D648
Vicat Softening Point 114 °C
237 °F
ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D542
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Transmission, Visible 92 %
92 %
ASTM D1003
Copyright © lookpolymers.com All Rights Reserved