Eurotec® Tecopet® PT70 GR30 NL100 MB PET, 30% glass fiber reinforced, impact modified, heat stabilized, natural

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer Eurotec
Trade Name Tecopet®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecopet® PT70 GR30 NL100 MB PET, 30% glass fiber reinforced, impact modified, heat stabilized, natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Eurotec®
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Moisture Absorption 0.200 %

@Temperature 23.0 °C
0.200 %

@Temperature 73.4 °F
50% RH; ISO 960
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
Eurotec
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
Eurotec
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 8.00 GPa
1160 ksi
ISO 527
Izod Impact, Notched (ISO) 9.00 kJ/m²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
11.0 kJ/m²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
[10 K/min], ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Comparative Tracking Index 250 V
250 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Processing Temperature 270 - 290 °C
518 - 554 °F
Feed Temperature 50.0 - 70.0 °C
122 - 158 °F
Throat
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 120 - 140 °C
248 - 284 °F
Dry Time 4.00 hour
4.00 hour
Moisture Content <= 0.080 %
<= 0.080 %
ISO 960
Hold Pressure 60.0 - 100 MPa
8700 - 14500 psi
Descriptive Properties Value Comments
Back Pressure Low
Injection Speed Fast