Eurotec® Tecomid® NA40 NL IH PA 6.6 impact modified

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Eurotec
Trade Name Tecomid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecomid® NA40 NL IH PA 6.6 impact modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good chemical resistanceGood flow and processing propertiesAPPLICATIONS: AutomotiveElectrical/ElectronicFurnitureConstructionHome appliances
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Filler Content 0.00 %
0.00 %
ISO 3451
Moisture Absorption at Equilibrium 2.0 %
2.0 %
Humidity Absorption, 50% RH, 23°C; ISO 62
Water Absorption at Saturation 6.0 %
6.0 %
23°C; ISO 62
Linear Mold Shrinkage 0.017 cm/cm
0.017 in/in
Linear Mold Shrinkage, Transverse 0.017 cm/cm
0.017 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527
Elongation at Yield 5.0 %
5.0 %
ISO 527
Tensile Modulus 1.50 GPa
218 ksi
ISO 527
Izod Impact, Notched (ISO) 20.0 kJ/m²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
85.0 kJ/m²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/eU
Charpy Impact, Notched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
9.00 J/cm²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
10 K/min; ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-1/2
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Comparative Tracking Index 600 V
600 V
IEC 60112