Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurotec® Tecolen® CP20 GR20 NL XC30 PPCP, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler , Polypropylene, Flame Retardant
Manufacturer Eurotec
Trade Name Tecolen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecolen® CP20 GR20 NL XC30 PPCP, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Eurotec®
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527
Elongation at Break 5.0 %
5.0 %
ISO 527
Tensile Modulus 4.00 GPa
580 ksi
ISO 527
Izod Impact, Notched (ISO) 25.0 kJ/m²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
[10 K/min], ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75
Flammability, UL94 V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Glow Wire Test 800 °C

@Thickness 2.00 mm
1470 °F

@Thickness 0.0787 in
GWIT; IEC 60695
850 °C

@Thickness 2.00 mm
1560 °F

@Thickness 0.0787 in
GWFI; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Processing Properties Metric English Comments
Processing Temperature 200 - 240 °C
392 - 464 °F
Feed Temperature <= 60.0 °C
<= 140 °F
Throat
Mold Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Hold Pressure 40.0 - 80.0 MPa
5800 - 11600 psi
Descriptive Properties Value Comments
Back Pressure Low
Injection Speed Medium - Fast
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved