Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurotec® Tecodur® PB70 KK45 NL XA 20 PBT 45% glass fiber/mineral reinforced, UL94 V0, low warpage

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Eurotec
Trade Name Tecodur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecodur® PB70 KK45 NL XA 20 PBT 45% glass fiber/mineral reinforced, UL94 V0, low warpage.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionGood dimensional stabilityVery good chemical resistanceExcellent flow and processing propertiesLow moisture absorptionVery good surface finishAPPLICATIONS: AutomotiveElectrical/ElectronicBusiness equipmentConstructionHome appliances
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
ISO 1183
Filler Content 45 %
45 %
ISO 3451
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Humidity Absorption, 50% RH, 23°C; ISO 62
Water Absorption at Saturation 0.25 %
0.25 %
23°C; ISO 62
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ISO 527
Elongation at Break 1.5 %
1.5 %
ISO 527
Tensile Modulus 10.0 GPa
1450 ksi
ISO 527
Izod Impact, Notched (ISO) 4.00 kJ/m²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eU
3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eU
Charpy Impact, Notched 0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 179/eA
0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10 K/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75-1/2
Vicat Softening Point 190 °C
374 °F
50N; ISO 306
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
plaque; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Comparative Tracking Index 300 V
300 V
IEC 60112