Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Eurostar Engineering Plastics
Trade Name Starpylen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starpylen MH0200A HDPE, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.91 g/cc
0.0690 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
on Tensile Bar; E2P method
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.0 MPa
2610 psi
5 mm/min; ISO 527
Elongation at Break 25 %
25 %
5 mm/min; ISO 527
Tensile Modulus 0.450 GPa
65.3 ksi
1 mm/min; ISO 527
Flexural Strength 33.0 MPa
4790 psi
2 mm/min; ISO 178
Flexural Modulus 0.300 GPa
43.5 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 195 - 205 °C
383 - 401 °F
Zone 2 215 - 225 °C
419 - 437 °F
Zone 3 225 - 250 °C
437 - 482 °F
Melt Temperature 225 - 250 °C
437 - 482 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Drying Temperature 70.0 °C

@Time 10800 sec
158 °F

@Time 3.00 hour