Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with Glass Fiber + Bead Filler
Manufacturer Eurostar Engineering Plastics
Trade Name Starpylen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Thickness 4.00 mm
0.0020 - 0.0040 in/in

@Thickness 0.157 in
E2P method
Melt Flow 3.0 - 10 g/10 min

@Load 5.00 kg,
Temperature 230 °C
3.0 - 10 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
5 mm/min; ISO 527
Elongation at Yield 1.5 %
1.5 %
5 mm/min; ISO 527
Tensile Modulus 5.60 GPa
812 ksi
1 mm/min; ISO 527
Flexural Strength 65.0 MPa
9430 psi
2 mm/min; ISO 178
Flexural Yield Strength 74.0 MPa
10700 psi
2 mm/min; ISO 178
Flexural Modulus 4.20 GPa
609 ksi
2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 195 - 205 °C
383 - 401 °F
Zone 2 215 - 225 °C
419 - 437 °F
Zone 3 225 - 250 °C
437 - 482 °F
Melt Temperature 225 - 250 °C
437 - 482 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Drying Temperature 70.0 °C

@Time 10800 sec
158 °F

@Time 3.00 hour