Eurostar Starpylen HZ 80E7 HDPE, Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Eurostar Engineering Plastics
Trade Name Starpylen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starpylen HZ 80E7 HDPE, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 2.55 g/cc
0.0921 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Elongation at Break >= 5.0 %
>= 5.0 %
5 mm/min; ISO 527
Elongation at Yield 14 %
14 %
5 mm/min; ISO 527
Flexural Yield Strength 28.0 MPa
4060 psi
2 mm/min; ISO 178
Flexural Modulus 4.40 GPa
638 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80x10x4; ISO 180/1U
Processing Properties Metric English Comments
Zone 1 195 - 205 °C
383 - 401 °F
Zone 2 215 - 225 °C
419 - 437 °F
Zone 3 225 - 250 °C
437 - 482 °F
Melt Temperature 225 - 250 °C
437 - 482 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Drying Temperature 70.0 °C

@Time 10800 sec
158 °F

@Time 3.00 hour