Eurostar Starpylen HU 70E4 ECR

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Eurostar Engineering Plastics
Trade Name Starpylen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Starpylen HU 70E4 ECR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Starpylen HU 70E4 ECR is a Renewable Calcium Carbonate (oyster shell) Masterbatch in a PP carrier. Engineered to reduce carbon footprint in mineral filled compound.Information provided by Eurostar.
Physical Properties Metric English Comments
Bulk Density 0.750 g/cc
0.0271 lb/in³
Internal
Density 1.67 g/cc
0.0603 lb/in³
ASTM D792
Filler Content 70 %
70 %
Renewable Mineral
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Thermal Properties Metric English Comments
Melting Point 162 °C
324 °F
ISO 3146
Processing Properties Metric English Comments
Drying Temperature 70.0 °C

@Time 14400 sec
158 °F

@Time 4.00 hour
Moisture Content 0.20 %
0.20 %